KOMPOSISYON SA KEMIKAL
incoloy 625 coiled tubing capillary tubing
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0.1 | 20 – 23 | ≥ 58 | ≤ 5 | ≤ 0.5 | ≤ 0.5 | 8 – 10 | ≤ 1* | ≤ 0.015 | ≤ 0.015 | ≤ 0.4 | 3.15 – 4.15 | ≤ 0.4 |
(mass%)
* Kung determinado
Alang sa ASTM B444, ASME SB444, AMS 5581
kahimtang | Kusog nga Tensile | Kalig-on sa ani | Elongation |
minimum, ksi | minimum, ksi | minimum,% | |
Grade 1 | 120 | 60 | 30 |
Grade 2 | 100 | 40 | 30 |
* Ang mas taas nga kusog nga mga kabtangan mahimong mahatag sa bugnaw nga gahi nga kahimtang.
70°F | 200°F | 400°F | 600°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Densidad | lbs/in3 | 0.305 | - | - | - | - | - |
Thermal Expansion | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Elastic nga Modulus | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Poisson Ratio | - | 0.278 | 0.28 | 0.286 | 0.29 | 0.295 | - |
Thermal Conductivity | Btu-in/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Piho nga Kainit | Btu/lb·°F | 0.098 | 0.102 | 0.109 | 0.115 | 0.122 | 0.118 |
Kalig-on sa ani | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Kusog nga Tensile | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 coiled tubing capillary tubing
PROSESODESCRIPTIONSteel MakingElectric Arc Furnace nga gisundan sa Vacuum Oxygen Decarburization (VOD) o Argon Oxygen Decarburization (AOD).Pipe MakingConventional Seamless Cold Finished Pipe and Tube Manufacturing Processes.Heat TreatmentDili matig-a pinaagi sa heat treatment.Mahimong ihatag sa annealed, solution annealed o cold hardened nga kondisyon.Ang mas taas nga kusog nga annealed nga kondisyon kasagarang gigamit sa mga serbisyo hangtod sa 1100 ° F, samtang ang solusyon nga annealed nga kondisyon gigamit sa mga aplikasyon nga labaw sa 1100 ° F.
Oras sa pag-post: Hul-06-2023